950-1050C (1742-1922F)

Metakaolin converts to spinel phase

As kaolin is calcined past the metakaolin stage (400-600C) it goes through an exothermic re-crystallization to form a spinel intermediate phase.

Related Information

Links

Temperatures Dehydroxylation in kaolin, ball clay (450-650)
Temperatures Spinel phase meta kaolin converts to mullite (1050-1200+)
Minerals Mullite
Mullite (3Al₂O₃·2SiO₂) is a naturally occurring aluminum silicate crystalline mineral. It forms in h
Materials Mullite
A highly refractory low-expansion alumino-silicate crystal formed naturally only rarely but produced industrially and within fired kaolin bodies.