Ferro Frit CC-266

Notes

Low COE. Early softening, late flow. Can stand alone or use to reduce crazing.

flow 1900
potassium oxide - <10
sodium oxide - <10
lithium dioxide - <10
aluminium oxide - 2-10
boron oxide - 15-30
silica - >50
C.E.O. - 5

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.